ZrO2+HfO2+Y2O3 ≥99% Y2O3 9%-10% Al2O3 <0.05% Density before sintering (g.cm-3) 3.20±0.05 Density after sintering (g.cm-3) 6.06±0.01 CTE (25-500°C) (K-1) 10.5±0.5

White Zirconia ST

تماس بگیرید
ZrO2+HfO2+Y2O3 ≥99% Y2O3 9%-10% Al2O3 <0.05% Density before sintering (g.cm-3) 3.20±0.05 Density after sintering (g.cm-3) 6.06±0.01 CTE (25-500°C) (K-1) 10.5±0.5

White Zirconia SHT

تماس بگیرید
ZrO2+HfO2+Y2O3 ≥99% Y2O3 9%-10% Al2O3 <0.05% Density before sintering (g.cm-3) 3.20±0.05 Density after sintering (g.cm-3) 6.06±0.01 CTE (25-500°C) (K-1) 10.5±0.5

White Zirconia HT-PLUS

تماس بگیرید
ZrO2+HfO2+Y2O3 ≥99% Y2O3 4.5% – 6% Al2O3 <0.25 Density before sintering (g.cm-3) 3.20±0.05 Density after sintering (g.cm-3) 6.06±0.01 CTE (25-500°C)

Coloring Liquid

تماس بگیرید
Temperature at Beginning(°C/(°F)) 450/842 Drying Time(min) 8 Heat rate (°C/°F per m) 55/131 Vacuum begins (°C/°F) 450/842 Vacuum ends (°C/°F)

فرز

تماس بگیرید
Materials Zirconia, Wax, PMMA, PEEK Cut Diameter Depends on your milling machine Shank Diameter Depends on your milling machine Overal

5D Multilayer

تماس بگیرید
ZrO2+HfO2+Y2O3 ≥99%   Y2O3 9%-10%   Al2O3 <0.05%   Density before sintering (g.cm-3) 3.20±0.05   Density after sintering (g.cm-3) 6.06±0.01

اسکنر داخل دهانی HELIOS 500 EIGHTEETH

580,000,000 تومان
  • ولتاژ ورودی: 5 ولت
  • جریان ورودی: 900 میلی آمپر
  • دارای دکمه برای تغییر حالت فک بالا، فک پایین و بایت
  • دارای منبع نور LED به همراه آینه ضدبخار
  • بدون نیاز به پودر
  • بدون نیاز به کابل جهت اتصال به پریز (استفاده از پورت USB برای انتقال اطلاعات و روشن شدن دستگاه)
  • امکان ذخیره داده ها در فضای ابری Eighteeth
  • امکان آپدیت نرم افزار به صورت اتوماتیک
  • کالیبراسیون خودکار